陕西省某金矿尼尔森选金试验研究
Study on Knelson Beneficiation of Gold Ore in Shanxi Province
投稿时间:2012-07-25  
DOI:
中文关键词: 金矿  重选  尼尔森选矿机  金回收率
英文关键词: gold ore  gravity separation  Knelson concentrator  gold recovery
基金项目:
作者单位E-mail
武俊杰 陕西省地质矿产实验研究所 starwjj555@126.com 
摘要点击次数: 4339
全文下载次数: 4668
中文摘要:
      针对陕西省某金矿的矿石性质,采用尼尔森选矿机对该矿石进行了重选回收金。试验结果表明,尼尔森一次选别金回收率达到87.38%,金精矿品位为233.3 g/t。与常规重选(摇床、溜槽)试验相比,简化了工艺流程,提高了金的回收率,为该金矿采用该重选设备提供了参考依据。
英文摘要:
      According to the characteristics of a gold ore in Shanxi province, the Knelson beneficiation equipment was applied to treat a coarse gold as a pre-recovery technology test. The results showed, the total recovery of gold arrived 87.38%, the recovery rate of gold concent was 233.3 g/t. Compared with conventional separation equipment (concentrating table, chute) trial, the processing flow sheet could simplify and improve gold recovery, which provides reference basis for adopting this type of equipment.