低品位微细粒金矿浮选精矿的处理工艺研究 |
Processing Technology on Low-grade Microgranular Gold Mine and Its Flotation Concentrate |
Received:June 06, 2014 |
DOI: |
中文关键词: 有色金属冶金 低品位微细粒金矿 高压氧化 氰化浸出 浸出率 渣率 |
英文关键词: nonferrous metallurgy low-grade microgranular gold mine high-pressure oxidation cyanide leaching leaching rate residue rate |
基金项目: |
Author Name | Affiliation | E-mail | XIE Yingbang | Guangxi Research Institute of Metallurgy, Nanning 530023, China | 13907713469@139.com | ZENG Rui | Guangxi Research Institute of Metallurgy, Nanning 530023, China | | LUO Siqiang | Guangxi Research Institute of Metallurgy, Nanning 530023, China | | ZHAN Haihong | Guangxi Research Institute of Metallurgy, Nanning 530023, China | | RONG Rong | Guangxi Research Institute of Metallurgy, Nanning 530023, China | |
|
Hits: 4687 |
Download times: 4678 |
中文摘要: |
针对低品位微细粒金矿中金的赋存特点,对其浮选精矿进行高压氧化-氰化浸出工艺处理。重点考察了高压氧化预处理过程中的温度、液固比和氧化时间对预处理效果的影响。预处理渣再磨后氰化浸出,金的浸出率(对浮选精矿)为94.30%,渣率为10.88%。 |
英文摘要: |
Considering the occurrence features of gold in low-grade microgranular gold mine, high- pressure oxidation-cyanide leaching process was used for treating its flotation concentrate. The effects of temperature, liquid-solid ratio and oxidation time, during the process of high-pressure oxidation, on pre- treatment were investigated crucially. The pretreatment slag was ground and leached with sodium cyanide. The leaching rate of gold, for flotation concentrate, was 94.30%, and the residue rate was only 10.88%. |
View Full Text
View/Add Comment Download reader |