加压碱溶法从氧化铝基废催化剂中回收钯 |
Recovery of Palladium from the Alumina-Based Waste Catalysts by Pressurized Alkali Dissolution Method |
Received:September 01, 2015 |
DOI: |
中文关键词: 有色金属冶金 钯 废催化剂 加压 碱溶 氧化铝 回收 |
英文关键词: nonferrous metallurgy palladium spent catalyst high pressure alkali solution aluminum oxide recovery |
基金项目:云南省省院省校科技合作项目(2013IB020)。 |
Author Name | Affiliation | ZHAO Yu | Sino-Platinum Metals Resources Yimen Co.Ltd., Kunming 651100, China | WANG Huan | Sino-Platinum Metals Resources Yimen Co.Ltd., Kunming 651100, China | HE Xiaotang | Sino-Platinum Metals Resources Yimen Co.Ltd., Kunming 651100, China | WU Xilong | Sino-Platinum Metals Resources Yimen Co.Ltd., Kunming 651100, China | LI Yong | Sino-Platinum Metals Resources Yimen Co.Ltd., Kunming 651100, China | LI Zixuan | Sino-Platinum Metals Resources Yimen Co.Ltd., Kunming 651100, China | LIAO Wei | Kunming Institute of Precious Metals, Kunming 650106, China | LEI Ting | Kunming Metallurgy College, Kunming 650033, China |
|
Hits: 2816 |
Download times: 3259 |
中文摘要: |
研究了加压碱溶载体法从氧化铝基含钯废催化剂中回收钯的工艺。在高压釜中,反应温度200℃,压力12 kg/cm2,时间6 h,氧化铝载体的溶解效率大于95%;选择甲酸钠作为抑制剂,可将钯在溶液中的浓度降低至0.0005 g/L以下;富集物经溶解-精炼得到纯度大于99.98%的海绵钯,钯直收率为99.02%。 |
英文摘要: |
The process of recovering palladium from the alumina-based waste catalysts by pressurized alkali dissolution method was studied. At the reaction temperature of 200℃, pressure of 12 kg/cm2, and the reaction time of 6 h in the autoclave, the dissolution efficiency of alumina carrier is more than 95%. With sodium formate as inhibitor, the concentration of palladium in solution can be reduced to less than 0.0005 g/L. By dissolving-refining the purity of sponge palladium could be reached to over 99.98%, and the direct recovery of palladium was 99.02%. |