Author Name | Affiliation | GAO Yiyuan | Sino-Platinum Metals Resources Yimen Co. Ltd., Yuxi 651100, Yunnan, China | YANG Shenhong | Sino-Platinum Metals Resources Yimen Co. Ltd., Yuxi 651100, Yunnan, China | WANG Biao | Sino-Platinum Metals Resources Yimen Co. Ltd., Yuxi 651100, Yunnan, China | WANG Huan | Sino-Platinum Metals Resources Yimen Co. Ltd., Yuxi 651100, Yunnan, China | WU Xilong | Sino-Platinum Metals Resources Yimen Co. Ltd., Yuxi 651100, Yunnan, China |
|
Hits: 771 |
Download times: 466 |
中文摘要: |
用王水对含铱树脂中的铱进行造液处理。实验表明,金属铱的溶解率可达90%,且金属基本不会损失。考察了王水浓度、加热温度、保温时间、料液比对于铱溶出率的影响;在王水浓度为80%,加热温度在85 ℃,保温时间为1.5 h,料液比为1:3的最佳条件下,金属铱的溶出率可达90%。 |
英文摘要: |
Use aqua regia to treat the iridium in the iridium containing resin. Experiments have shown that the dissolution rate of metal iridium can reach 90%, and the metal will not be lost. The effects of aqua regia concentration, heating temperature, holding time, and material liquid ratio on the dissolution rate of iridium were investigated; Under the optimal conditions of 80% aqua regia concentration, heating temperature at 85 ℃, holding time of 1.5 hours, and a material liquid ratio of 1:3, the dissolution rate of metallic iridium can reach 90%. |